POLYNOR DIY+PRO 65 High quality mounting foam

₽735
In stock
Color: from white to gray
Using temperature: from -10 ° C to +35 ° C *
Ballon temperature: from +15 ° C to +25 ° C
Film formation time: 6-15 min. **
Preliminary time? Processing: 35-60 min. **
Full staining time: 24 hours
Thermous?
Density: 23-25 ​​kg/m3
Size stability (shrinkage): 3 - 5% ***
Water absorption: 1.5% (after 24 hours)
Compression force: 0.03 MPA
Stretching force: 0.14 MPa
Thermal conductivity: 0.032 W/m*K
Solvents (before foam hardening): Polynor Cleaner

* (optimum temperature +23 ° C)
** (at a temperature of +23 ° C and air humidity 35%)
*** (at a temperature of +23OC, air humidity 35%, within 24 hours)

High performance
Does not support combustion
Excellent adhesion to a large spectrum of building materials

Homogeneous, fine -handed structure
High acoustic and thermal insulation
Cutting start 35-60 min.
Foundations for mold and moisture
Distinctive feature - density 23-25 ​​kg/m3
Secondary extension up to 25 %
Shelf life - 12 months

Other products from this supplier

123
Universal Polynor Foam 60 seconds Universal foam
The universal Polynor foam 60 seconds is designed for high-q
₽790
In stock,
delivery from Moscow
95
Mounting foam 70 Mega Therm
High -quality Polynor 70 MEGA Therm One -component polyureth
₽750
In stock,
delivery from Moscow
99
POLYNOR THERMOBLOCK adhesive
POLYNOR RUSSLAND LLC offers to wholesale POLYNOR THERMOBLOCK
₽690
In stock,
delivery from Moscow
107
POLYNOR 65 PREMIUM high quality mounting foam
POLYNOR RUSSLAND LLC sells high-quality POLYNOR 65 PREMIUM p
₽700
In stock,
delivery from Moscow
Show all products from this supplier